【摘 要】
:
Amorphous phosphor 1.4Y2O3·2.5Al2O3·0.1Tb2O3 (the same composition as Y2.8Tb0.2Al5O12) was prepared via a sol-gel method at relatively low temperature (i.c.,
【机 构】
:
College of Chemistry and Chemical Engineering,Beijing National Laboratory for Molecular Sciences,Sch