Gleeble 2000热模拟实验机上采用变形开始的同时喷水淬火和减少变形量的方法,对形变诱导铁素体的形成机制进行了一系列实验研究实验研究表明,形变导致了铁素体的块型相变和针状铁素体的相变析出,同时在奥氏体温区形变诱导铁素体在变形后具有不稳定、自发逆相变的特点 A series of experimental studies on the formation mechanism of deformation-induced ferrite have been carried out on the Gleeble 2000 thermal simulator by means of water quenching and deformation reduction at the beginning of the deformation. Experimental results show that the deformation causes the ferrite bulk phase Phase transformation and acicular ferrite precipitation, while deformation in the austenite temperature zone induced deformation of ferrite instability, spontaneous reverse phase change
其他文献
提出了预测三元系合金中原子浓度(原子分数,%)低于10的组元的扩散系数、本征扩散系数和热力学因子的模型;通过此模型预测1473 K时,Ni-Al-Cr(富Ni)三元合金系的扩散系数,并和
In order to prevent cracking appeared in the work?piece during the hot stamping operation, this paper proposes a hybrid optimization method based on Hammersley
基于电磁离心凝固过程温度场的数值模拟结果,建立了铸件凝固过程物理参数与铸件凝固组织之间的定性关系通过计算固/液界面前沿液相温度梯度 G与界面生长速度 R之间的比值(G/R)及冷却速
为连续监测常温下金属中氢浓度,根据 Devanathan—Stachurski电池原理设计了一种新型的双电极电化学氢传感器,采用电镀 Ni层作为催化剂,金属氧化物电极作为辅助电极用电化学方法和 SEM研究厂背景电流问题
在钢线热镀 Cu实验基础上,建立简化的动态数学模型,模拟反向凝固的工艺过程,研究主要工艺参数影响的规律,以模拟参数的形式描述界面处的接触热阻,合理地反映了铜液和钢芯之间的热交
研究了金属间化合物合金 Ni-20Al--30Fe的超塑性行为及其机理结果表明,该合金的显微组织由 β相和 γ/γ’相组成;在 102──1253 K, 1.67×10-4—3.34×10-3 S-1拉伸变形时,合金呈超塑性,最大伸长率可达 469%. SEM分析发现超塑性变
利用磁控溅射技术制备了Fe含量(质量分数,%)分别为25和50的两种Fe-Cu纳米涂层,并研究了该涂层在700与 800 ℃空气中的氧化结果表明, Fe—75Cu涂层氧化后形成了外层为氧化铜和内侧为氧化铁的复合氧化膜,而 Fe—
笔者以1984-2009年发表在国内外期刊上的关于BAF研究与应用的多篇文献为基础,对曝气生物滤池中的同步硝化反硝化作用从宏观、微观和微生物角度进行机理分析,并从DO、C/N、pH
High bonding strength, low deformation and convenient procedure are all very important aspects in the microfluidic device fabrication process. In this paper, an
选取退火45钢为研究对象,考察冲击接触载荷下亚表层微观形变特征与损伤结果表明,冲击接触载荷下,铁素体的变形以多沿移为特征;滑移在品界受阻产生应力集中并产生力偶使晶粒发生相对