用离旋加选择性絮凝的湿法选矿工艺,可将SiO2含量为75%左右的团田中位硅藻土的品位提高到SiO2>85%以上,达到高品位的水平。用此精矿加工的助滤剂的滤速4.30-5.26ml/cm2·min,过滤效果好,其它指标符合食品助滤剂要求。
With the spin-selective flocculation of the wet beneficiation process, the SiO2 content of about 75% of the Central Valley diatomite grade increased to SiO2> 85%, reaching high levels. With this concentrate processing filter aid filtration rate 4.30-5.26ml / cm2 · min, filtering effect, and other indicators in line with food filter aid requirements.