The grain oriented silicon strip was rolled by cross shear rolling(CSR)and then annealed to manufacture non-oriented thin silicon strip of high quality.The recrystallization of rolled grain-oriented silicon steel into non-oriented silicon steel was studied.For this purpose,CSR is better than conventional rolling,and the higher the mismatched speed rate is,the better the properties of the non-oriented thin silicon strip are.The optimum annealing schedule is heating at 1 000 ℃for 1hin pure hydrogen atmosphere added with H2 S of 0.001 0 %.
The grain oriented silicon strip was rolled by cross shear rolling (CSR) and then annealed to manufacture non-oriented thin silicon strip of high quality. The recrystallization of rolled grain-oriented silicon steel into non-oriented silicon steel was studied. For this purpose , CSR is better than conventional rolling, and the higher the mismatched speed rate is, the better the properties of the non-oriented thin silicon strip are. The optimum annealing schedule is heating at 1 000 ° C. for 1 hin pure hydrogen atmosphere added with H2 S of 0.001 0%.