为了使钼粉得到较高的密度,将其在2500K的高温下进行烧结。而添加2wt%Ni或5wt%Ni3Al粉末的钼粉,在1573K下保温1h进行烧结时,其密度分别达到94%和96%。也就是说,添加Ni粉或Ni3Al合金粉末显著地提高了钼粉的烧结特性。日本熊本大学机械工程与材料科学系的M. Nishida等人采用?
In order to obtain a higher density of molybdenum powder, it is sintered at a high temperature of 2500K. The molybdenum powder with 2wt% Ni or 5wt% Ni3Al powder sintered at 1573K for 1h had a density of 94% and 96%, respectively. That is, adding Ni powder or Ni3Al alloy powder significantly improves the sintering characteristics of the molybdenum powder. M. Nishida et al., Department of Mechanical Engineering and Materials Science, Kumamoto University, Japan