Ti–Mo alloys with various Mo contents from 6wt% to 14wt% were processed by spark plasma sintering based on elemental powders.The influence of sintering tempera
(Mg66.2Zn28.8Ca5)100-xCux(at%,x = 0,1,3,and 5) bulk metallic glasses(BMGs) of 2 mm in diameter were prepared by the conventional copper mold injection casting m
Stoichiometric pure and tellurium(Te) doped indium bismuthide(InBi) were grown using the directional freezing technique in a fabricated furnace.The X-ray diffra