Ni-SDC相关论文
用溶胶一凝胶法制备了Ce0.8Sm0.2O2-δ(SDC)和SmCo0.6Feo0.2-XNiXO3(x=0,0.1,0.2)(SCFN)系列纳米粉体并烧结为陶瓷片,用XRD、TEM、......
The SmBaCuMO5+δ (M=Fe,Co,Ni) (SBCM) powders were synthesized by the citrate sol-gel method and the powders were sintere......